By using mechanical energy aided aluminizing process, an aluminized layer of 20~180μm was obtained on titanium plate at a low temperature of 650~700°C for 3 hours. The aluminized layer consists of an outer layer of single-phase aluminium, an inner layer of (Al,Si)3Ti intermetallic compound and aluminium bipolar layer, the silicon element is riched in the Al3Ti intermetallic compound.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.