Air plasma spraying system was utilized to deposit Ni3Al coatings on AISI 321 steel samples. After plasma spraying the coatings were heat treated at different temperatures i.e. 500 °C to 800 °C for 10 to 100 hours. The characterization tools such as, X-Ray diffraction analysis, optical and scanning electron microscopy were used. By comparing the XRD scan data of as sprayed and heat treated coating, it was observed that the formation of NiO increases drastically with time and temperature. Due to the formation of NiO, hardness was also enhanced. The oxidation behavior was observed by using optical microscope and when it was studied that the oxidation was increasing with time and temperature. Further, the SEM tool was utilized to study the detail microstructural behavior such as shrinkage cavity and oxide particles. The other phases like alumina and spinel phases were determined by using Energy dispersive spectrometer method.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call