The effect of micron-size silicon nitride (Si3N4) particles additions, up to 1.0 wt. % on Sn-Cu-Ni (SN100C) solder alloy was investigated. Sn-Cu-Ni composite solder were prepared via powder metallurgy (PM) technique. Different percentages of Si3N4(0, 0.25, 0.5, 0.75 and 1.0 wt. %) were added into the alloy. Result revealed that reinforcement was well distributed between the grain boundaries which could positively affect the properties of the composite solder.