Abstract
Microstructural evolution of the brazed Ti–6Al–4V and TZM joint using 95Ag–5Al braze alloy was studied. The Ti–6Al–4V substrate is well wetted by the molten braze at 900 °C. However, the TZM substrate cannot be wetted by the molten braze, even if the brazing temperature is increased to 950 °C. The brazed joint is comprised of the Ag-rich phase alloyed with Al and Ti. There is almost no interfacial reaction between the molten braze and TZM. On the other hand, the Ti–6Al–4V substrate reacts with the molten braze and formed TiAl interfacial layer. The growth of TiAl reaction layer can be significantly inhibited by the application of infrared brazing.