Abstract
The knowledge of the microstructural evolution during exposure to high temperatures is important to understanding the mechanisms responsible for the creep resistance of silicon carbide (SiC) ceramics. This includes not only the phase transformation of the SiC grains, but also the phase transformations of the oxynitride grain‐boundary phases. For this study, a series of SiC specimens were prepared with varying molar ratios of AlN‐Y2O3 additives. Increased creep resistance was observed in specimens with an additive system containing a 2:3 molar ratio or 60 mol% Y2O3. A continuous oxide layer of Y2Si2O7 formed at the surface during elevated temperature testing in air. No blistering or cracking was observed in this oxide coating. Further increase of the creep resistance was achieved by a post‐sintering nitrogen anneal.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.