Abstract

By studying the static birefringence pattern of cadmium telluride electro-optic modulator crystals after fabrication, it has been determined that standard fabrication processes induce excessive stress birefringence. This stress birefringence is produced during the grinding stage of fabrication. Two methods for removing this birefringence have been explored: (1) mechanical polishing of the sides of the crystal to an optical finish, and (2) chemical etching of the sides of the crystal with a 5% bromine solution. Both methods reduced the static birefringence of the crystal. The stress birefringence pattern can be recreated by grinding the sides of the crystal with 9 μm polishing grit.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.