Abstract

The fracture toughness of soda-lime glass was measured by applying thermal stresses to center-cracked plates. Mode I cracking was achieved by chilling the crack faces. The stress intensity factor was obtained by combining temperature measurements with a finite element solution. The average value of KIC = 0.77 MN/m3/2 based on three tests agrees well with values in the literature for a water-free environment. Mode II cracking was achieved by applying a temperature gradient normal to the crack. A value KIIC = 1.6 MN/m3/2 was obtained in two tests using a finite element computation based on the temperature distribution computed from the specimen’s thermal boundary conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.