Abstract
A test of lithium wettability was performed in high vacuum (< 3 × 10(-4) Pa). High magnification images of Li droplets on stainless steel substrates were produced and processed using the MATLAB(®) program to obtain clear image edge points. In contrast to the more standard "θ/2" or polynomial fitting methods, ellipse fitting of the complete Li droplet shape resulted in reliable contact angle measurements over a wide range of contact angles. Using the ellipse fitting method, it was observed that the contact angle of a liquid Li droplet on a stainless steel substrate gradually decreased with increasing substrate temperature. The critical wetting temperature of liquid Li on stainless steel was observed to be about 290 °C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.