Abstract
A bioleaching study aimed at recovering metals from hazardous spent hydroprocessing catalysts was carried out. The exhaust catalyst was rich in nickel (4.5 mg/g), vanadium (9.4 mg/g) and molybdenum (4.4 mg/g). Involved microorganisms were iron/sulphur oxidizing bacteria. Investigated factors were elemental sulphur addition, ferrous iron addition and actions contrasting a possible metal toxicity (either adding powdered activated charcoal or simulating a cross current process by means of periodical filtration). Ferrous iron resulted to be essential for metal extraction: nickel and vanadium extraction yields were 83% and 90%, respectively, while about 50% with no iron. The observed values for molybdenum extraction yields were not as high as Ni and V ones (the highest values were around 30-40%). The investigated actions aimed at contrasting a possible metal toxicity resulted not to be effective; in contrast, sequential filtration of the liquor leach had a significant negative effect on metals extraction. Nickel and vanadium dissolution kinetics resulted to be significantly faster than molybdenum dissolution ones. Furthermore, a simple first order kinetic model was successfully fitted to experimental data. All the observed results supported the important role of the indirect mechanism in bioleaching of LC-Finer catalysts.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.