Abstract
The tensile strengths of bulk solders and joint couples of Sn-3.5Ag-0.5Cu, Sn-3.5Ag-0.07Ni, and Sn-3.5Ag-0.5Cu-0.07Ni-0.01Ge solders and the shear strengths of ball grid array (BGA) specimens, solder-ball-attached Cu/Ni/Au metallized substrates were investigated. The tensile strength of the bulk is degraded by thermal aging. The Ni-containing solder exhibits lower tensile strength than Sn-3.5Ag-0.5Cu after thermal aging. However, the Ni-containing solder joints show greater tensile strength than the Cu/Sn-3.5Ag-0.5Cu/Cu joint. Fracture of the solder joint occurs between the intermetallic compound (IMC) and the solder. The shear strength and fracture mechanism of BGA specimens are the same regardless of solder composition.