Abstract

This work is an assessment of the mechanical reliability of Au and Cu ball bonds to Al, Ni/Au and Ni/Pd/Au surfaces in terms of high temperature storage. All systems show very good shear strength after thermal storage for up to 120 days at 150 °C. The Au ball bonds on Al surface show Kirkendall voiding starting from 60 days. This did not decrease their mechanical strength but it is expected to become a reliability issue in the long run. The Cu wire bonds on Al caps show a higher initial strength, much slower intermetallics formation and no Kirkendall voiding. This makes them a potentially better industrial solution. Excellent bond strength was found for Cu- and Au-bonds on Ni/Au and Ni/Pd/Au caps. No intermetallics formation or other microstructural change have been found on these interfaces up to 120 days at 150 °C, which was related to the full solubility of the materials along these interfaces. This result suggests that they can be a successful industrial solution for the next generation of packages.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.