Abstract

The effect of curing conditions (sealed and standard) on the mechanical properties of fly ash (FA) and ground-granulated blast-furnace slag (GGBFS)–based alkali-activated materials with NaOH and waterglass alkali activators are investigated in this study. The results show the highest 28-day compressive strength of samples was obtained in the A-3 samples and researched to 59.8 MPa under sealed curing conditions. Using scanning electron microscopy (SEM), it was found that samples with sealed curing condition have higher mechanical properties associating to the denser microstructure and low crack width. Under the sealed curing condition, lower carbonation degree of samples has higher content of Na+ to form the Si-O-Na bond resulting in the higher content of amorphous gel and geopolymerization degree based on the experiments results of electron paramagnetic resonance (EPR), Fourier transform infrared (FTIR) spectrometer, X-ray photoelectron spectroscopy (XPS), chemical bond water, and selective dissolution.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.