Thermoelectric (TE) modules are exposed to temperature gradients and repeated thermal cycles during their operation; therefore, mechanically robust n- and p-type legs are required to ensure their structural integrity. The difference in the coefficients of thermal expansion (CTEs) of the two legs of a TE module can cause stress buildup and the deterioration of performance with frequent thermal cycles. Recently, n-type Mg3Sb2 and p-type MgAgSb have become two promising components of low-temperature TE modules because of to their high TE performance, nontoxicity, and abundance. However, the CTEs of n-Mg3Sb2 and p-MgAgSb differ by approximately 10%. Furthermore, the oxidation resistances of these materials at increased temperatures are unclear. This work manipulates the thermal expansion of Mg3Sb2 by alloying it with Mg3Bi2. The addition of Bi to Mg3Sb2 reduces the coefficient of linear thermal expansion from 22.6 × 10-6 to 21.2 × 10-6 K-1 for Mg3Sb1.5Bi0.5, which is in excellent agreement with that of MgAgSb (21 × 10-6 K-1). Furthermore, thermogravimetric data indicate that both Mg3Sb1.5Bi0.5 and MgAgSb are stable in air and Ar at temperatures below ∼570 K. The results suggest the compatibility and robustness of Mg3Sb1.5Bi0.5 and MgAgSb as a pair of thermoelectric legs for low-temperature TE modules.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.