Poly-ether-ether-ketone( PEEK) coatings with different melt indexes( MI) were prepared on the stainless steel substrate via electrostatic powder spraying method. Amorphous coatings were obtained by quenching the as-melted coatings into the ice-water medium. Semi-crystalline coatings were obtained by annealing the amorphous coatings in an oven for 30 min at 260 ℃. The XRD results indicates that the structure of PEEK coatings transforms from amorphous to semi-crystalline via the treatment of annealing. The hardness and the behavior friction of the PEEK coatings were tested. The result demonstrates that by the same treatment,the PEEK coatings with larger MI have higher crystallinity. The semi-crystalline PEEK coatings have higher hardness,lower friction coefficient and better wear rate than the amorphous ones. The poor fluidity of PEEK-A with lower MI leads to the rough coatings. Both of the PEEK-B and PEEK-C with larger MI can form smooth coatings and the friction coefficients and wear rates of them are stable. The friction coefficients of semicrystalline coatings B and C are less than 0. 15,and the wear rates are less than 20 ×10-6mm3/( N·m). Therefore PEEK with larger MI is more suitable for the preparation of PEEK coating by electrostatic spraying.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.