This study evaluated the effects of different concentrations of benzalkonium chloride (BAC) on the preservation of adhesive interfaces created with two etch-and-rinse adhesives and its inhibitory properties on dentin matrix metalloproteinase (MMP) activity. The following groups were tested with the adhesive systems Optibond Solo Plus and All-Bond 3: Group 1, adhesive without inhibitor (control); Group 2, topical 2.0% chlorhexidine (2.0% CHX); Group 3, phosphoric acid with 1.0%wt BAC (BAC-PA); Group 4, 0.25% BAC-adhesive (0.25% BAC); Group 5, 0.5% BAC-adhesive (0.5% BAC); Group 6, 1.0% BAC-adhesive (1.0% BAC); and Group 7, 2.0% BAC-adhesive (2.0% BAC). Composite cylinders were fabricated, and shear bond strength (SBS) was evaluated after 24 h, 6 months, and 18 months of storage. Extracts from concentrated demineralized human dentin powder were subjected to SDS-PAGE and incubated in the presence of 0.25, 0.5, 1.0, and 2.0% BAC. Overall, stable bonds were maintained for 18 months. Improved bond strengths were seen for 0.5% BAC and 1.0% BAC when bonding with Optibond Solo Plus, and for 0.25% BAC and 0.5% BAC when bonding with All-Bond 3. Zymographic analysis revealed complete inhibition of gelatinolytic activity with BAC. Benzalkonium chloride, at all concentrations, inhibited dentin proteolytic activity, which seems to have contributed to the improved bond stability after 18 months for specific combinations of BAC concentration and adhesive.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.