In the current study, a factorial design is used to investigate the effect of total iron and silica on the metallurgical performance of different grades of manganese ores. The derived mathematical formulations are applied to estimate the reduction disintegration index (RDI+6.3, RDI+3.15, and RDI−0.5), reduction index (total reduction index (RIT), manganese reduction index (RIM), and iron reduction index (RIF)), and softening-melting property (start of softening (TS1), end of softening (TS2), start of melting (Tm1), and end of melting (Tm2)) of manganese ores. The RDI+6.3 and RDI+3.15 are increased with the individual effect of SiO2 and the interaction effect of iron with silica, while they are decreased as the total iron increased. The high-Fe high-SiO2 manganese ore showed the highest RIT and RIF. The RIM was almost identical in all manganese ores. The presence of high content of SiO2 resulted in a narrow softening range (62–83°C), while the high-Fe high-SiO2 manganese ore exhibited a wider softening range (135–140°C). The melting range was very small in high-Fe low-SiO2 (3–16°C) and high-Fe high-SiO2 (6–8°C) manganese ores, while the low-Fe low-SiO2 manganese ore showed wider melting range (72–74°C). The derived mathematical models are in a good agreement with the experimental results. The calculations are carried out using Matlab program.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.