Material attractiveness analysis on isotopic plutonium compositions of fast breeder reactors (FBR) has been investigated based on figure of merit (FOM) formulas as key parameters as well as decay heat (DH) and spontaneous fission neutron (SFN) compositions. Increasing minor actinide (MA) doping gives the significant effect to increase Pu-238 composition. However, the compositions of Pu-240 and Pu-242 become less with increasing MA doping. DH and SFN compositions in the core regions similar to the DH and SFN compositions of MOX-grade. Material attractiveness based on FOM1 formula shows all isotopic plutonium compositions in the blanket regions as well as in the core regions are categorized as high attractive material. Adopted FOM2 formula can distinguishes the material attractiveness levels which show the plutonium compositions in blanket regions as high attractiveness level and its composition in the core regions as low level of material attractiveness. MA doping is effective to reduce the material attractiveness level of blanket regions from high to medium and it requires much more MA doping rate to achieve low level of attractiveness (FOM<1) based on adopted FOM1 formula. Low material attractiveness level can be obtained by 4 % or more doping MA based on adopted FOM2 formula which considers not only DH composition effect, but also SFN composition effect that gives relatively higher contribution to material barrier of plutonium isotopes.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call