Abstract

Martensitic transformation in off-stoichiometric Co2VSi Heusler alloy was firstly confirmed in this work. The martensite phase presents an ordered 2M non-modulate D022 structure transformed from L21 Heusler structure. In the Co63.5V17.0Si19.5 alloy, the forward and reverse martensitic transformation temperatures are extremely high which reach up to 683°C and 693°C, respectively, higher than most known Heusler-type high-temperature shape memory alloys. And results also indicate that the single martensite phase alloy exhibits a good ductility and strength with the compressive strain of over 15% and strength of about 2300MPa, respectively. What's more, the recoverable strain being maximal to around 3.1% can be obtained at high temperature (750–800°C) due to its reverse martensitic transformation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.