Abstract

Both Ti/APC-2 cross-ply and quasi-isotropic nanocomposite laminates were successfully fabricated. Basically, the tensile tests at elevated temperature were conducted to obtain the baseline data of mechanical properties, such as strength and stiffness. The results for both types of laminates of longitudinal stiffness predicted by the rule of mixtures (ROM) were in good agreement with experimental data, whilst, those ultimate strength predicted by ROM were lower than the measured data. Then, the tension-tension (T-T) constant stress amplitude cyclic tests were performed at elevated temperature to receive the S-N curves, fatigue strength and life. It is a surprise that almost no delaminations were observed in tensile and cyclic tests, even at elevated temperature and over a million cycles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.