Amorphous Fe 100- x B x (11.5 ≦ x ≦ 22) alloys having the invar characteristics were prepared by a single roller quenching method to investigate the magneto-volume effect. Forced volume magnetostriction, ∂ω/∂ H, increased remarkably with decreasing boron content and the maximum value obtained was about 90 × 10 −10 Oe −1 at 11.5 at.% boron. The estimated value of the pressure dependence of the Curie temperature, ∂ T c /∂ P, was considerably large, being comparable to those of crystalline FeNi invar alloys. The ∂ T c /∂ P curve plotted as a function of T c approximately fitted Wohlfarth's expression.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.