Abstract

The dependence of reduced remanence (Mr/Ms) and coercivity of Sm22Co78/Fe65Co35 bilayer and Sm22Co78/Fe65Co35/Sm22Co78 triple-layer films on Fe65Co35 soft-magnetic layer thickness d, was systematically investigated. All the hysteresis loops of the films exhibited a single-phase behavior, reflecting a strong exchange coupling between soft-and hard-magnetic phase. Mr/Ms showed a monotonic increase with increasing Fe65Co35 thickness d, and the coercivity would show a peak with increasing d. From the plot of M versus applied field H, it is shown that the positive profile decreases and the negative interaction profile increases with the increase of interfaces between soft-and hard-layers.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.