Abstract

In this work we investigated the photoluminescence properties of Y2O3:Er3+, Eu3+ as a function of temperature and the possibility to use this material as a temperature sensor. Photoluminescence emission measurements with 532 nm laser excitation were recorded in the temperature range from 303 up to 573 K. The measured intensity ratio of erbium 4S3/2 → 4I15/2 and europium 5D0 → 7F2 emission lines was used for determination of the temperature calibration curve. These emission lines are intense, narrow and well defined. The distance between the lines, being 47 nm, can be easily measured even with a low-resolution spectrometer. The calculated relative sensitivity of the temperature sensor was 1.4% K−1 at 303 K, in the physiological temperature range, meaning that it could be successfully applied in biological studies.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.