Abstract

The dielectric constants of lead iron niobate (PFN) and 40% lead zinc niobate (PZN) added to lead iron niobate (PFN 0.6-PZN 0.4) have been measured as a function of pressure up to 6 GPa under isothermal conditions between room temperature and 348 K. The relaxor transition temperature measured at 1 kHz excitation frequency varies at a rate −24.5 K/GPa for PFN and at a rate of −28.8 K/GPa for the PFN 0.6-PZN 0.4 composition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.