An investigation of low temperature reactive ion etching of silicon to produce ultrasmall structures is presented. Etching was performed between 10–100 mTorr with SF6/O2 plasmas. The silicon samples were cooled using liquid nitrogen, allowing the temperature to be controlled over the range of +25 to −120 °C. With a flow rate of 1 sccm of SF6 and sample temperatures below −85 °C the etch produces nearly anisotropic etching in agreement with predictions of the reactive spot model. At higher flow rates etching produced facetted features indicating higher chemical reactivity of the plasma with the silicon. With the addition of O2 to the plasma the facetting became even more pronounced.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.