Abstract

Several device concepts have been further evaluated after the successful implementation of epitaxial Si, SiGe and/or Si:C layers. Most of the next device generations will put limitations on the thermal budget of the deposition processes without making concessions on the epitaxial layer quality. In this work we address the impact of ex-situ wet chemical cleans and in-situ pre-epi bake steps, which are required to obtain oxide free Si surfaces for epitaxial growth. The combination of defect measurements, Secondary Ion Mass Spectroscopy, photoluminescence, lifetime measurements, and electrical diode characterization gives a very complete overview of the performance of low-temperature pre-epi cleaning methods. Contamination at the epi/substrate interface cannot be avoided if the pre-epi bake temperature is too low. This interface contamination is traceable by the photoluminescence and lifetime measurements. It may affect device characteristics by enhanced leakage currents and eventually by yield issues due to SiGe layer relaxation or other defect generation. A comparison of state of the art 200 mm and 300 mm process equipment indicates that for the same thermal budgets the lowest contamination levels are obtained for the 300 mm equipments.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.