Abstract

The surface oxidation of a titanium oxynitride (TiOxNy) film after long-time storage of 25 month in ambient conditions is investigated. The TiOxNy film is prepared by plasma-enhanced atomic layer deposition using tetrakis(dimethylamino)titanium and nitrogen plasma, and the film is characterized by Ar+ ion sputtering of the film surface in combination with x-ray photoelectron spectroscopy (XPS) as well as by angle-resolved XPS. The total thickness of an oxygen-enriched layer at the surface of the TiOxNy films is found to be about 0.7 nm and it consists of a sequence of a 0.4 nm thick TiON/TiO2 enriched layer followed by a 0.3 nm thick TiO2 enriched layer underneath compared to the bulk composition of the film which shows constant values of 29% TiN, 29% TiO2, and 42% TiON. The results suggest that the TiON enrichment takes place initially at the surface followed by a surface and subsurface oxidation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.