The reliability of a pure silica core single-mode fiber with long-term exposure to continuous wave (CW) high-power laser light is reported. It is found that the optical loss in the 0.6-1.6-μm region and the Raman spectrum remain unchanged after 1900 h of exposure to 8-W CW laser light at 1.48 μm. The nonbridging oxygen hole center concentration generated by 1900 h of exposure is estimated to be below our detection limit of 2×10/sup 12/ cm/sup -3/.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.