Abstract
We demonstrate the thermally actuated phase change of VO2 films formed by atomic layer deposition and subsequent thermal annealing on InAlN/AlN/GaN heterostructures. To locally raise the device temperature above the VO2 semiconductor–metal transition temperature, a two-dimensional electron gas formed within the InAlN/AlN/GaN heterostructure was used as an integrated resistive heater. An ON/OFF resistance ratio of nearly 103 was achieved for 50 nm VO2 films over a temperature range of 25 to 105 °C. The time required to switch the VO2 film from high- to low-resistance states was shown to depend on the applied heater power, with sub-microsecond transition times achieved.