AbstractWith lower alloying cost and higher mechanical properties, lean duplex stainless steels can be an alternative to the more commonly used austenitic stainless steels. However, these alloys are still not the preferred choice, probably due to a lack of field experience. A study was thus initiated in view of defining the limits of use of selected (lean) duplexes for urban wastewater treatment units. The present paper shows the localized corrosion performance of selected lean duplexes in chloride contaminated solutions. The results are compared with austenitic S30403 and S31603 and with the more standard duplexes S82441 and S32205. The effect of welding was also investigated. Exposures in field municipal wastewater plants were conducted for 1 year in low and high chloride content units. The results show that lean duplexes S32101 and S32202 can be used as alternatives to S30403 and S31603 in low chloride electrolytes. At 500 ppm of chloride content, duplex stainless steel S32304 showed better corrosion resistance than S30403 and S31603. For higher chloride contents (1000 ppm and above) the standard duplexes S82441 and S32205 shall be preferred.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call