Abstract

Abstract Pure lead soldered to the gage section of 200-ksi (1379-MPa) 4145 steel tensile specimens tested at temperatures ranging from room temperature to 700°F (371°C) exhibit a severe loss in ductility between 400 and 680°F (204 and 360°C). The ductility, as measured by reduction of area, recovered at 695°F (368°C), the so-called brittle-to-ductile recovery temperature. This recovery temperature was shifted to higher temperatures in a sensitive manner by relatively small amounts of either tin or antimony added to alloy the externally applied lead.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.