Abstract

Line edge roughness (LER) and line width roughness (LWR) are analyzed during pattern transfer in a self-aligned quadruple patterning (SAQP) process. This patterning process leads to a final pitch of 22.5nm, relevant for N7/N5 technologies. Measurements performed by CD SEM (Critical Dimension Scanning Electron Microscope) using different settings in terms of averaging, field of view, and pixel size are compared with reference metrology performed by planar TEM and three-Dimensional Atomic Force Microscope (3D AFM) for each patterning process step in order to investigate the optimal condition for an in-line LWR characterization. Pattern wiggling is als0 quantitatively analyzed during LER/LWR transfer in the SAQP process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.