Abstract
The influence of Mo addition on pitting corrosion resistance of lean duplex stainless steels is not clearly understood in alkaline chloride conditions even if this element is widely recognized to increase corrosion resistance in acidic and neutral environments. This work aims to study the effect of Mo on pitting corrosion of lean duplex stainless steels in synthetic concrete pore solutions simulating degraded concrete. Results are discussed with respect to the influence of Mo on pitting potential for two industrial alloys in chloride rich and carbonated solution simulating concrete pore environments. To establish the real effect of Mo addition on lean duplex corrosion and passivation properties, two specific laboratory lean duplex alloys, for which the only difference is strictly the Mo content, are also studied. Mo presented a strong positive influence on the pitting corrosion resistance of industrial and laboratory lean duplex stainless steels in all studied chloride-rich solutions, but its effect is as less pronounced as the pH increases. In presence of Mo, pitting initiates and propagates preferentially in the austenitic phase at high temperature.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have