Abstract

In this study, the applicability of leaching and CIL processes in gold recovery with thiourea method, alternative to the cyanidation from the refractory Gümüşhane-Kaletaş/Eastern Black Sea Region (Turkey) ore was investigated. The experiments were conducted at laboratory conditions using ore samples of which approximately 80% were ground to −0.038 mm. The grade of the ore samples was 6.8 g Au/ton. At the first part of the experimental studies, assuming that the gold could be recovered with CIC and CIP processes, the effects of pH, thiourea, oxidizing agent consumption, and leaching time on leaching were investigated. Then, on the basis of the optimum pH and reagent consumption values obtained in the first part (pH = 1.5, 15.2 kg thiourea/ton ore, 140.9 kg iron(III) sulfate/ton ore and 46.2 kg sulfuric acid consumption/ton ore) and adding 50 kg activated carbon/ton ore at the beginning of experiments, the gold leaching extents were obtained for the same leaching times. At this part, the applicability of CIL process in gold recovery with thiourea was investigated for the first time. As a result of the experiments, although higher gold leaching extents were obtained in CIL process, the increase in extent was about maximum 8% and the highest gold leaching extent was obtained as 75% at the end of the 5th hour.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.