Abstract

Transmission laser welding using Incremental Scanning Technique(TWIST) mode and conventional contour welding mode were adopted to investigate laser transmission welding of 0.5mm thick PET plate. A 1064nm fiber laser was used to weld PET at the (TWIST) mode, and an 808nm diode laser was applied to conduct the conventional contour welding. The Clearweld coating was used as laser absorbing material. The influences of laser parameters (i.e. defocusing distance, distance between two circles) on the quality of weld seams were analyzed by optical microscopy. Moreover, geometry and shear strength of the weld zone were tested to optimize laser parameters. Additionally, the water vapor permeability (WVP) of weld seams was measured to test hermetical capacity. Results show that the shear strength and hermetic capacity of weld seam by TWIST mode are at the same level in comparison with that of the conventional contour welding.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.