Abstract
At the Chair of Timber Constructions of the Swiss Federal Institute of Technology in Lausanne (EPFL) tests were carried out to join wooden work pieces by friction welding without any additional welding deposit. It could be determined that this kind of technology, which is mainly used for thermoplastics and metal, can also be applied to wood. Tests were carried out to determine the influence of the processing parameters like welding pressure, frequency and amplitude of the circular movement on the welding process and the input of energy at the interface. In addition, the resistance of the joint was examined. The development of the shear strength during solidification of the interface as well as the shear strength achievable after a complete solidification of the interface was the objective of the examinations. Furthermore, the microstructure of the welded joint was studied to reveal the manner in which the thermally decomposed wood forms the connection between the welded pieces.
Submitted Version (Free)
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.