Abstract

A nodular cast iron (German designation GGG) sewer pipe leaked within a short time of use (13 years). The pipe was destroyed by sulphuric acid induced corrosion. Microbes form hydrogen sulphide and further oxidation leads to H2SO4. Sewer pipes are coated inside with a protective alumina cement layer, which was attacked firstly, followed by a corrosion of cast iron. Spongiose is a corrosion of cast iron, thereby ferrite is destroyed and graphite and cementite are remaining unattacked. Spongiose is observed commonly in grey cast iron, but is unusual for nodular cast iron. The alumina cement coated GGG tube, the corrosion products and their different graduations were investigated. In the corroded spongiose-layer the crystalline phases graphite, cementite, hematite and magnetite were identified. In the rust-layer deposits of lepodocrocite and goethite are the main phases but also sulphur, gypsum and other sulphuric compounds were observed.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call