The influence of hydrothermal aging on the structural stability of Cu-modified SAPO-34 prepared by ion-exchange and impregnation methods was studied. XRD, Ar adsorption at −196 °C, solid-state NMR, UV–vis, H2-TPR, and EPR were used to probe the structural properties of the catalysts. It was found that the precipitation of crystalline AlPO4 and SiO2, the appearance of mesopores, the migration of silicon to form siliceous islands, and the formation of copper oxide crystallites occurred in aged catalysts. Furthermore, more siliceous islands and copper oxide crystallites were present in the aged samples prepared by the impregnation method than in those prepared by the ion-exchange method. Therefore, the impregnated catalysts show a much poorer structural stability than the ion-exchanged catalysts, which leads to more serious deterioration in the NH3-SCR reaction after hydrothermal aging.