Abstract
Abstract In order to improve the mechanical properties of the W–Cu alloy, the W–Cu–Zn alloys with low W–W contiguity were fabricated by three different preparation methods. For the first method, the mixed powder of copper-coated tungsten powder and Zn powder was sintered by SPS (Spark Plasma Sintering) process. For the second method, the mixed powder was processed by CIP (Cold Isostatic Pressing) before SPS. For the third method, a skeleton of the copper-coated tungsten powder was prepared by CIP, and then the skeleton was infiltrated with H70 brass. The microstructure, mechanical properties and failure mechanism of the prepared W–Cu–Zn alloys were investigated. The results show that the W–Cu–Zn alloy fabricated by the third method achieves a high relative density of 98.4% and a low W–W contiguity of 10%. The alloy exhibits a high dynamic compressive strength of 1000 MPa, with a high critical failure strain of 0.7. The Cu-Zn matrix of the alloy fabricated by the third method is composed of α-phase Cu–Zn alloy and Cu3Zn particles. The homogeneous distribution of Zn in the matrix manifests good solution strengthening effect and the uniformly distributed Cu3Zn particles has a strong precipitation strengthening effect, which are both responsible for the evidently enhanced mechanical properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.