Abstract

The wheel topographies in the different stages during grinding fused silica and BK7 were measured on machine with a white light interferometer. Height parameters of 3D surface roughness, including maximum peak height, standard deviation, skewness and kurtosis, were proposed to evaluate the wheel wear mechanisms during grinding the two types of optical glasses. The results show that wheel wear mechanisms are essentially determined by different material removal modes. BK7 and fused silica were predominantly ground in ductile mode and brittle mode respectively. The grinding of BK7 mainly causes severe attritious wear of grains. During grinding fused silica, self-sharpening effect makes grinding sustain for a long time.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.