Abstract

This study presents the investigation of TiB distribution characteristics on the microstructure of in-situ synthesized TiB/Ti6Al4V single-track composites manufacture with laser metal deposition. Ti6Al4V alloy was reinforced by adding TiB2ceramic at mass volumes of 0%, 1% and 2% for microstructure modification and mechanical properties enhancement. The TiB/Ti6Al4V composite was characterized using optical microscope (OM), scanning electron microscope (SEM), electron backscatter diffraction (EBSD) and microhardness. It was found that the addition of TiB2resulted in the transformation of the prior β-grain into two types of morphologies of dendritic and columnar microstructures. Furthermore, the increase in the amount of TiB2resulted in the reduction of the volume fraction of β-Ti phase, with the in situ formed TiB replacing and occupying the β-Ti positions. Deposition at 2% promoted the formation of unmelted TiB2particles which promoted hardness increase to 496 ± 17 HV.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.