ABSTRACT The distribution of residual stresses (RS) in repairs generated by Friction Hydro-Pillar Processing (FHPP) in AISI H13 was investigated. Three axial force levels, with consequent different deposition rates, were applied to replicate possible repaired conditions. The contour (CM) and X-ray diffraction (XRD) methods were employed for RS analysis in samples that were also evaluated through metallography, microhardness analysis, micro-tensile and Charpy testing. CM produced 2D maps of the RS in the joints, showing symmetrical distributions around the welded rod for all welded conditions. Other common features for all conditions were the maximum level of compressive RS, which was found in the TMAZ of the rod, and the maximum tensile residual stress, which was found near the HAZ of the base block. There was good agreement between the RS measurement techniques. Mechanical tests show similar tensile resistance for all conditions and an apparent increase in toughness at higher force levels.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.