Abstract
The 0.5 mm thickness ultra-thin sheets of 6061-T4 Al and T2 Cu were butt joined by micro friction stir welding under different ω/ν. When the ω/ν was 36, the welding process resulted in a defect-free joint. This joint exhibited the highest tensile strength (222 Mpa), which was similar to the Al BM. This joint failed in the heat-affected zone on the Al side, where the hardness was lowest, leading to a ductile fracture. When the ω/ν was 9, the welding process led to the formation of agglomerated intermetallic compounds (IMCs) in upper nugget zone (NZ), and the IMCs layer of Al2Cu and Al4Cu9 developed in lower NZ. Therefore, the joint strength was greatly weakened, resulting in failure at the Al/Cu interface. The fracture mode of the joint exhibited a mixture of ductile and brittle behaviors.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.