Abstract

Positron lifetime spectra of the semicrystalline polymer Polytetrafluoroethylene (PTFE) with high amorphous content are measured between — 190°C and 420°C and are decomposed into four annihilation terms. The four positron lifetimes and intensities reflect, apart from their density-caused temperature dependence, the structural changes of the polymer at the first and second order transitions. Above 100°C a secondary crystallization can be clearly observed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.