Abstract

Present research work was focused to investigate the firing temperature effects on mineralogical phase composition of nine clay bricks collected from the brick factory of Kathmandu valley using X-ray diffraction (XRD) patterns and Fourier transform infrared (FTIR) spectra analyses. Main mineralogical phases of quartz, feldspars, spinel, mullite and hematite in the brick specimens fired at different firing temperatures including muscovite type of mica mineral in the sun-dried brick specimen are identified from XRD and FTIR analyses. Disappearance of the muscovite type of mica clay mineral with feldspars enhanced to form alumina rich spinel phase at firing 900° to 1000° C, and finally the primary mullite phase in the fired clay brick samples is clearly observed at 1100° C firing temperature.BIBECHANA 16 (2019) 122-130

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.