Abstract

Pickling, sizing, and descaling of Zircaloy with HF leaves firmly bound fluorine on the surface. This deposit can be determined by proton activation utilizing the 19F(p,αγ)16O reaction. The method described herein involves comparing gamma-ray yields from the sample and a comparative standard. The errors inherent in comparing targets of different thicknesses of deposit (hence, different effective cross sections) are calculated. As little as 0.01 µg/cm2 can be determined. The total thickness can be obtained simply. Some results for nuclear reactor components and test coupons are given.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.