Abstract

The magnetic field dependence of filling factors has been investigated on InP based In053Ga047As/In052Al048As quantum well samples with two occupied subbands by means of magnetotransport measurements at the temperature of 15K in a magnetic field range of 0 to 13T. Under the condiction that Laundau-level broadening is larger than the spin splitting of each subband, filling factors are even when the splitting energy of two subbands is an integer multiple of the cyclotron energy, i.e.ΔE21=kωc. If the splitting energy of two subbands is half of an odd interger multiple of the cyclotron erergy, i.e.ΔE21=(2k+1)ωc/2, the filling factor is odd.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.