Abstract

Chemical leaching is one of the most efficient methods for improving low-grade coal due to its ability to remove both inorganic and organic minerals economically. This study examined the qualitative demineralisation using the XRD and FTIR analyses. Moreover, microcrystalline analysis was investigated by analysing the Micro-Raman spectra, and ash composition was analysed using XRF Spectroscopy analysis for coal samples. Furthermore, a correlation was established between a Raman parameter (AD/AG) and a crystallite parameter (Lc). The demineralisation mechanism was postulated in light of the findings to explain how significant impurities (SiO2 and Al2O3) with iron-bearing elements (Fe2O3 and FeS2) were curtailed during multi-stage leaching. The maximum deashing and demineralisation were obtained by treatment with 40% (w/v), i.e. 10 M NaOH, followed by HCl with HNO3 solution in a 3:1 ratio, with an average particle size of 180 μm. 79% ash reduction and 48% enhancement in GCV were achieved compared to raw coal.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call