A promising plasma enhanced atomic layer deposition (PEALD) Cu process has been developed, and PEALD Cu layers have been investigated for use in multilevel damascene metallization. Continuous and conformal PEALD Cu layers as thin as 12 nm were deposited on blanket and high aspect ratio patterned substrates. The effects of hydrogen plasma pretreatments on the material and integration properties of the PEALD Cu process have been studied. Plasma pretreatments were observed to improve Cu nucleation and enable lower Cu resistivity and surface roughness. Void-free electrochemically deposited Cu fill was achieved on PEALD Cu-seeded high aspect ratio via structures. The plated Cu films possess a strong (111) texture inherited from the PEALD Cu seed layer.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.