Abstract

This letter presents a new strategy for the formation of continuous Cu seed layer in high aspect ratio (HAR) through-silicon-vias (TSVs) with large depth based on sequential sputtering and electroless plating. The deposited seed layer is continuous and dense even at the bottom of the TSVs, which is difficult to achieve by individual sputtering or electroless plating. Combined with the spin coating of polyimide (PI) liner, atomic layer deposition (ALD) of TiN barrier layer, and electroplating of Cu conductor, TSVs with diameter of <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$9~\mu \text{m}$ </tex-math></inline-formula> and depth of <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$141~\mu \text{m}$ </tex-math></inline-formula> are successfully fabricated, and the aspect ratio is 15.5. The TSVs are fully filled without cracks or voids, proving the good quality of seed layers. Electrical measurements show that the minimum capacitance of a single TSV is around 145 fF, and the leakage current is about 3.4 pA at 20 V, indicating good electrical properties of the fabricated TSVs and the feasibility of the proposed fabrication flow in deep HAR TSV applications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.