The morphology of β-Mg17Al12 phase and corrosion behavior of AZ91HP magnesium alloy after spheroidizing treatment were investigated by optical microcope electrochemical and immersion tests in 3.5% NaCl at 25°C. The results show that the coarse divorced eutectic phase of AZ91HP cast magnesium alloy dissolve into Mg matrix during the isothermal process at 415°C, and the lameller β phase precipitated from magnesium solid solution as perlite-type precipitation during the slowly cooling. Next, the spheroidizing treatment at different temperatures for 20h was carried out, and the lameller β phase were spheroridizing by dissolved themselves. After spheroidizing treatment at 300°C for 20h, many small granular β phase are scattering within the magnesium matrix. The corrosion properties of AZ91HP magnesium alloy in 3.5% NaCl decreased obviously after spheroidizing treatment, the polarization measurement of the alloy can be up to -1.412V from -1.56V of the cast. The β-Mg17Al12 phase act as a corrosion barrier and hinder corrosion propagation, if the second phase is in the form of a spherical morphology.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.